Introduction to products
PRODUCT NAME SLJ42 Chlorinated Rubber deck paint
BRIEF One Pack water paint made from chlorinated rubber, modifier,pigments and extenders
FEATURES
-Good adhesion, high hardness and abrasion
-High chlorine content, has good flame retardancy and mildew resistance
-Excenllent water resistance, corrosion resistance and permeability resistance
-Construction is not restricted by seasonal temperatures
RESISTANCE GUIDE
HEAT RESISTANCE Up to 65℃ dry heat
WEATHERABILITY Excellent
SOLVENTS Resists splash and spillage of aliphatic solvents and mineral oil
ACIDS Resists splash and spillage of most inorganic acid fluid
ALKALIS Resists splash and spillage of most alkalis
SALTS Resists splash and spillage of most alkali salts
WATER Resists splash and spillage of fresh and salt water.
ABRASION Excenllent
USES:Widely used on ship deck; deck and floor of offshore facility and mining machinery
TYPICAL PROPERTIES AND APPLICATION DATA
COLOR Colors
DENSITY 1.3g/cm3
SOLIDS BY VOLUME 42%
SOLIDS BY WEIGHT 70%
SPREADING RATE 5.3 m2/kg (60um DFT)
DRYING TIME(23℃) Touch 4 Hr Handle 24 Hr
OVERCOAT INTERVAL(23℃) Min 4 Hr Max none
STORAGE at least 12 months (dry, cool and under cover )
PACKAGING 22kg
DIRECTIONS Before using stir or using dynamic mixer mixing two components completely. Rate of cure will vary depending on temperature and other factors such as ventilation, film thickness, humidity, thinner. The temperature of stir will >15℃, otherwise thinner should be added for needed viscosity after stir. Overmuch thinner will lead sag and slow cure rate, thin film, thinner should beadded after mixed. Practical spreading rates may be reduced 5%—25% for wastage of different application conditions.
APPLICATION
STEEL: The surfaces coated by primer or intermediate paint must be dry and clean,
remove oil, grease and other pollutants When overcoat on a two-component primer, wharf's pavement quality for old film or high-pressure water injection processing
should be taken if more than the longest accordance with time.
Don’t apply at temperatures below -10℃ or above 40℃. Don’t apply at relative humidity above 85% or when the surface is less than 3℃ above the dew point. In construction of lower than 0 ℃, the coated surface shall be free of ice, snow, etc
Don’t apply if there is fog, rain, snow or strong wind.
BRUSH/ROLLER: Suitable for small areas only. Apply even coats of the mixed material to the prepared surface. Thin if necessary with up to 0-15% with X-3 Thinner X-3. Additional coats may be required to attain specified thickness.
CONVENTIONAL SPRAY: Thinning is not normally required, however 0-15% of Chlorinated Rubber Thinner X-3 can be added.
AIRLESS SPRAY: Thinning is not normally required, however 0-5% of Chlorinated Rubber Thinner X-3 can be added. Pump ratio is 23:1 or 32:1 and fluid tip is 0.38-0.43 mm.
Overcoating: Aged coating should be tested for lifting by a method such as ‘X’cut or crosshatch methods. If it lifts, remove it. The surface must be free of oil, grease and other contaminants.
Previous coat: Epoxy Coatings, Chlorinated Rubber Coatings
CLEAN UP: with Chlorinated Rubber Thinner X-3
SAFETY: Pay attention to the safety precautions before and after using this product. Users should comply with the provision of the respective country or local government. It’s dangerous or deadly to eating it. To avoid inhalation of thinner steams and spray mists.
Use protective wears correctly; the skin and eyes should avoid contacting it. Use with good ventilation. This product is flammable. All sources of ignition must be eliminated in, or near the working area. DO NOT SMOKE. Fight fire with foam, CO2 or dry chemical powder. On burning will emit toxic fumes.
Notes: The data in the manual is get from standard experiments and may be vary from different conditions in use. Please refer to the latest manual if the data is altered and we would not inform specially.